Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY 522 PC/PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 265 °C
12 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
chs 2.0 in/min; ASTM D638
Flexural Modulus 2.036 GPa
295.3 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 6.94 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
13.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256