DSM Stanyl® TW271F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Lubricated + Glass Fiber Reinforced
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TW271F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by DSM Engineering Plastics.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
(DAM); ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527-1/-2
Elongation at Break 7.0 %
7.0 %
ISO 527-1/-2
Tensile Modulus 4.10 GPa
595 ksi
ISO 527-1/-2
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 295 °C
563 °F
(DAM); ISO 11357-1/-3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
IEC 60093