Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure

Category Polymer , Rapid Prototyping Polymer
Manufacturer DSM Somos
Trade Name NanoTool™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavily filled with non-crystalline nanoparticles allowing for faster processing. It exhibits superior side wall quality, along with excellent detail resolution as compared to other composite stereolithography materials.ApplicationNanoTool's smooth surface quality and high initial modulus make it an excellent resin for metal plating, a growing application which saves time and money as an alternative to fully metal prototypes. It's also ideal for creating strong, stiff parts that need to resist high temperatures, including wind tunnel models for aerospace and automotive applications. A third major application area is rapid tooling for injection molding.Information Provided by DSM Desotech Inc.
Physical Properties Metric English Comments
Density 1.65 g/cc

@Temperature 25.0 °C
0.0596 lb/in³

@Temperature 77.0 °F
Water Absorption 0.23 %
0.23 %
ASTM D570-98
Viscosity 2500 cP

@Temperature 30.0 °C
2500 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 94
94
ASTM D2240
Tensile Strength, Yield 61.7 - 78.0 MPa
8950 - 11300 psi
ASTM D638M
Elongation at Break 0.70 - 1.0 %
0.70 - 1.0 %
ASTM D638M
Tensile Modulus 11.0 - 11.4 GPa
1600 - 1650 ksi
ASTM D638M
Flexural Strength 79.0 - 121 MPa
11500 - 17500 psi
ASTM D790M
Flexural Modulus 10.2 - 10.8 GPa
1480 - 1570 ksi
ASTM D790M
Poissons Ratio 0.34 - 0.38
0.34 - 0.38
ASTM D638M
Izod Impact, Notched 0.120 - 0.150 J/cm
0.225 - 0.281 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear 25.3 - 26.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
14.1 - 14.4 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
30.4 - 32.4 µm/m-°C

@Temperature 0.000 - 50.0 °C
16.9 - 18.0 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
75.9 - 87.4 µm/m-°C

@Temperature 50.0 - 100 °C
42.2 - 48.6 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
90.0 - 95.7 µm/m-°C

@Temperature 100 - 150 °C
50.0 - 53.2 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 85.0 - 90.0 °C
185 - 194 °F
ASTM D648-98c
Glass Transition Temp, Tg 57.0 - 62.0 °C
135 - 144 °F
ASTM E1545-00
Electrical Properties Metric English Comments
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
ASTM D150-98
3.9

@Frequency 1000 Hz
3.9

@Frequency 1000 Hz
ASTM D150-98
4.0

@Frequency 60.0 Hz
4.0

@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 15.6 - 16.8 kV/mm
396 - 427 kV/in
ASTM D149-97a
Descriptive Properties Value Comments
Appearance Off White
Dp (mm) 0.11
Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2) 84
Exposure that gives 0.254mm thickness
Ec (mJ/cm2) 8.3
Critical exposure
Users viewing this material also viewed the following: