Material Notes:
Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental food contact can occur. ANDEROL 6000 Series Fluids are made for use in gear sets, bearings, circulating oil systems and chain applications. The heavier viscosity grades provide excellent service in worm gear units. ANDEROL food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.”Information provided by ConocoPhillips.Anderol® is a registered trademark of The Anderol Company.
Physical Properties Metric English Comments
Specific Gravity 0.860 g/cc
0.860 g/cc
60°F; ASTM D-1298
Viscosity Measurement 125
125
Viscosity Index; ASTM D-2270
Saybolt Viscosity at 100°F 996 SUS
996 SUS
ASTM D-2161
Saybolt Viscosity at 210°F 107 SUS
107 SUS
ASTM D-2161
Kinematic Viscosity at 40°C (104°F) 215 cSt
215 cSt
ASTM D-445
Kinematic Viscosity at 100°C (212°F) 22 cSt
22 cSt
ASTM D-445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
ASTM D-2783
Four Ball Wear 0.400 mm
0.0157 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
Thermal Properties Metric English Comments
Pour Point -35.0 °C
-31.0 °F
ASTM D-97
Flash Point 224 °C
435 °F
ASTM D-92
Descriptive Properties Value Comments
Copper Corrosion 1A
3 hrs. at 100°C, ASTM D130
Rust Test Pass
ASTM D665A