Compuestos Dominicanos Polycom AM-440495 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Compuestos Dominicanos, S.A. (polycom)
Trade Name Polycom
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Compuestos Dominicanos Polycom AM-440495 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance. Applications: Wire covering for fence Appearance: Green pelletsInformation provided by Compuestos Dominicanos
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.39 g/cc
1.35 - 1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86 - 88

@Time 15.0 sec
86 - 88

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 19.7 MPa
2850 psi
ASTM D412
Elongation at Break 315 %
315 %
ASTM D412