Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories CRMG-S02 Long Stopper

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CRMG-S02 Long Stopper.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.42 g/cc
0.0874 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.004905 GPa

@Temperature 1400 °C
0.7114 ksi

@Temperature 2550 °F
0.005886 GPa

@Temperature 23.0 °C
0.8537 ksi

@Temperature 73.4 °F
Compressive Strength 31.4 MPa
4550 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 5.20 µm/m-°C

@Temperature 1000 °C
2.89 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 3.0 %
3.0 %
MgO 68 %
68 %
SiO2 1.0 %
1.0 %
Descriptive Properties Value Comments
Chemical Analysis(%),FC+SiC 24+1
Remarks For erosive steel