Category | Polymer , Adhesive , Thermoset , Polyurethane, TS |
Manufacturer | ITW Devcon |
Trade Name | Flexane® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 g/cc | 0.0426 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 87 | 87 | Cured; ASTM D2240 |
Tensile Strength at Break | 11.7 MPa | 1700 psi | ASTM D412 |
Elongation at Break | <= 300 % | <= 300 % | ASTM D412 |
Tear Strength | 52.6 kN/m | 300 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 280 | 280 | H-18 wheel (1000 gram load) |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
82.2 °C | 180 °F | dry | |
Shrinkage | 0.14 % | 0.14 % | Cured; ASTM D2566 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 720 min | 12.0 hour | Functional cure |
Pot Life | 20.0 min @Temperature 23.9 °C |
20.0 min @Temperature 75.0 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Coverage per pound, in² @ 1/4" thickness | 94 | |
Mix ratio by weight (Resin:Hardener) | 72:28 |