ChevronTexaco Superla® 38 White Oil

Category Fluid , Lubricant , White Mineral Oil (WMO)
Manufacturer ChevronTexaco Corp
Trade Name Superla®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Superla® 38 White Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly chemically inert oils are virtually free of nitrogen, sulfur, oxygen and aromatic hydrocarbons. Chevron Superla White Oils contain Vitamin E, a natural antioxidant, to protect quality during handling and storage. They are clear, bright, and free of solids and water.ApplicationsChevron Superla White Oils find wide application:where direct food contact may occurwhere prolonged contact with human skin is necessarywhere odor and staining must be minimizedwhere outstanding long service under adverse conditions is requiredChevron Superla White Oils must be stored in approved containers to prevent contamination that could jeopardize their food grade status.
Physical Properties Metric English Comments
Specific Gravity 0.868 g/cc
0.868 g/cc
API Gravity 30.6 °
30.6 °
Saybolt Viscosity at 100°F 390 SUS
390 SUS
Kinematic Viscosity at 40°C (104°F) 76 cSt
76 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 232 °C
450 °F
ASTM D92
Descriptive Properties Value Comments
Color +30 minimum, Saybolt