| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil Teresstic 100
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil Teresstic 460
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil 32 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
|
|||
| Pour Point | <= -12.0 °C | <= 10.4 °F | ASTM D97 |
|
ExxonMobil Mobiltherm 43
Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems. It has a high specific heat an..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil SAE 30 Mobilgard ADL Series
Mobilgard ADL Series by ExxonMobil is a high performance family of increased dispersancy engine oils for high BMEP medium and high-speed diesel engines operating on distillate and MDO fuels. These a..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco 10-T White Oil
FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | |
|
ChevronTexaco 2190 T-EP Military Symbol Oil
Texaco Military Symbol Oil 2190 T-EP delivers value through:Long lubricant life because of selected base stocks and additives.Extreme pressure characteristics that provide high film strength to prot..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | |
|
ChevronTexaco 22 White Oil
Texaco White Oils 22 delivers value through:Nonstaining — Colorless, odorless, tasteless and nonstaining. The purity of Texaco White Oil 22 makes it the preferred choice for applications calling fo..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco Gear Compounds EP, ISO 1000
FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure
protection, antiwear and demulsibility, oxidation, rust, corrosion control an..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco ISO 1000 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco ISO 320 Machine Oil AW
FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco ISO 680 AIO
FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring ..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco ISO 680 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | See Note 3. |
|
ChevronTexaco Molytex® EP NLGI Grade 0
Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle ..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | See Note 3. |
|
ChevronTexaco Molytex® EP NLGI Grade 2
Texaco Molytex EP grease delivers value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading, extending vehicle ..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | See Note 3. |
|
ChevronTexaco Multifak® AFB NLGI Grade 2
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | See Note 3. |
|
ChevronTexaco Multifak® EP NLGI Grade 1
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | |
|
ChevronTexaco Regal® Marine 77
Texaco Regal Marine 77 delivers value through:Long lubricant life because of selected base stocks and additivesExtreme pressure characteristics provide high film strength to protect gears and bearin..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco RPM® NLGI 2 Heavy Duty LC Grease EP
FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco Superla® DCO
FeaturesChevron Superla DCO is a highly refined food grade white mineral oil that exceeds FDA purity requirements for the dedusting of grains intended for human consumption.Chevron Superla DCO conta..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | |
|
ChevronTexaco Vanguard® 1000
Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p..
|
|||
| Pour Point | <= -12.0 °C | <= 10.4 °F | ASTM D97 |
|
ExxonMobil Febis K Series 32
Exxon Febis K Series oils are premium quality lubricants designed to satisfy the strictest requirements of machine tool slideways. Their multi-functional performance makes them suitable for combined..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil Teresstic 100
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil Teresstic 46
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ExxonMobil Teresstic M Series 32HT
The Teresstic M Series of products is the latest addition to the family of Teresstic turbine lubricant products, long recognized for their high quality and reliability. Teresstic M Series are design..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco Clarity® ISO 320 Paper Machine Oil
FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOS..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco Sil-X® NLGI 1 Grease
FeaturesChevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.It is transpare..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | See Note 3. |
|
ChevronTexaco Starplex® NLGI Grade 1
Texaco Starplex greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protectio..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco Superla® 18 White Oil
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch..
|
|||
| Pour Point | -12.0 °C | 10.4 °F | ASTM D97 |
|
ChevronTexaco AFP White Oil
Chevron White Oil AFP is a technical grade white oil processed from paraffinic oilApplicationsChevron White Oil AFP’s major application is the dedusting of animal feeds and the preparation of anima..
|
|||