ChevronTexaco ParaLux™ 6001 Paraffinic Process Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name ParaLux™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco ParaLux™ 6001 Paraffinic Process Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with superior physical and chemical properties :lower aromatics result in superior color stability.Lower volatility improves efficiency.Excellent compatibility with rubber polymers reduces processing headaches.ApplicationsBecause PARALUX is produced by all-hydroprocessing, it has performance properties that surpass most conventional paraffinic process oils and approach or surpass many of the performance characteristics of technical white oils. These advantages include:Exceptionally low aromatic contentBetter color and UV stability than conventional paraffinic or naphthenic oilsAlmost complete resistance to degradation from ultraviolet discolorationLower volatility results in fewer emissions, so less make-up oil is needed and costs are minimizedExcellent compatibility with rubber polymers which require paraffinic oils. Only all-hydroprocessed oils can deliver all of these advantagesChevron ParaLux Process Oils are ideal for use in compounding a wide variety of products, including :FootwearAgricultural SprayFurniture PolishTextilesWire and Cable insulationAdhesives, sealants and coatingsPolymer modified asphaltsAsphalt extenderAutomobile interior moldingsAutomotive under hood partsTires, tire whitewalls, tubes, and inner linersInsulationGelsDielectric FluidsDrilling FluidsCarpet UnderlaymentHeat transfer fluidsFoamHousehold productsRoofing compoundsRubber membranesWeather Stripping
Physical Properties Metric English Comments
Specific Gravity 0.8718 g/cc
0.8718 g/cc
API Gravity 30.8 °
30.8 °
Viscosity Measurement 0.7946
0.7946
Viscosity Gravity Constant
Saybolt Viscosity at 100°F 606 SUS
606 SUS
Saybolt Viscosity at 210°F 70 SUS
70 SUS
Kinematic Viscosity at 40°C (104°F) 116 cSt
116 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 12.5 cSt
12.5 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 275 °C
527 °F
ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4781
1.4781
Descriptive Properties Value Comments
21 CFR 178.3620 ( c ) Pass
Aniline Point °F 254
Aromatics, by HPLC, % <1
Carbon Type by n-d-m, % Naphthenic 30
Carbon Type by n-d-m, %Aromatic 0
Carbon Type by n-d-m, %Paraffinic 70
Color +25, Saybolt
Saturates, by HPLC, % >99