Material Notes:
FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure protection, antiwear and demulsibility, oxidation, rust, corrosion control and foam inhibition.Chevron Gear Compounds EP used in misting systems provide excellent oxidation stability to prevent oil mist deposits. They will form a high volume of mist droplets for transmission to the point of application. Chevron Gear Compounds EP have minimal stray mist (fog).ApplicationsChevron Gear Compounds EP are recommended for all industrial enclosed gearing and wherever an AGMA extreme pressure lubricant is specified.Chevron Gear Compounds EP, in the proper viscosity grade, are recommended for all mist oil application systems.The same products can also be used in general industrial plant lubrication where the performance properties of this type of lubricant are required.
Physical Properties Metric English Comments
API Gravity 31.3 °
31.3 °
Viscosity Measurement 100
100
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 495 SUS
495 SUS
Saybolt Viscosity at 210°F 64 SUS
64 SUS
Kinematic Viscosity at 40°C (104°F) 95 cSt
95 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 11 cSt
11 cSt
ASTM D445
Mechanical Properties Metric English Comments
Timken Test 29500 g
65.0 lb
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Flash Point 225 °C
437 °F
ASTM D92
Descriptive Properties Value Comments
FZG Gear Wear Test, Failure Load Stage 12