Nye Lubricants 723GR-BLUE (RL) Rheolube Grease

Category Fluid , Lubricant , Lithium Gellant , Organic Soap Gellant , Polyalphaolefin (PAO)
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nye Lubricants 723GR-BLUE (RL) Rheolube Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 220
220
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 73 cSt
73 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
Base Oil; ASTM D445
Evaporation Loss 0.20 %
0.20 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 331
331
ASTM D217
Penetration P(60), 1/10 mm 344
344
ASTM D217
Oil Separation 5.2 %
5.2 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -40.0 °C
-40.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type Li soap