Saint-Gobain Transflow® M-34-R Raw Milk Tubing Formulation

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Transflow®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Saint-Gobain Transflow® M-34-R Raw Milk Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Transflow M-34-R: Transflow Raw Milk tubing is specially formulated to reduce the risks that can occur with the use of rubber tubings. Many regulatory sanitarians throughout the world recognize Transflow as the preferred tubing for raw milk transfer. Long lasting Transflow tubing is extremely flexible and installs quickly and easily around stantions and milk handling equipment. It resists embrittlement and cracking from oxidation that often shortens the service life of other tubings. The same reliability and performance found in Transflow Raw Milk tubing is also available for tank truck operators. Produced in large bore sizes up to 3” I.D., Transflow tubings' clarity, flexibility and cleanability are ideally suited for bulk milk transfer. Transflow is also produced in single and twin tube confiations ideally suited for supply air transport. It&#39s smooth inner surface is less susceptible to particle entrapment which can restrict air flow while crystal clarity permits detection of equipment deficiencies such as backflow of milk into the air lines. Every foot of Transflow Raw Milk tubing has been embedded with a trademark blue stripe within the tubing walls. The embedded blue stripe is your assurance of receiving genuine Transflow tubing, the worlds&#39 finest raw milk tubing produced specifically for the dairy industry.Features/Benefits:Excellent clarity for visual inspection of milk flowSmooth, non-porous bore resists buildupTaste and odor freeLightweight and flexible for quick installationNon-wetting properties allow easy cleaning and complete drainageLong and reliable service lifeMeets FDA, 3-A and NSF criteriaUsed primarily for Raw Milk Transport Lines.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792-91
Water Absorption 0.14 %
0.14 %
24 hours at 23°C; ASTM D570-81
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
15 seconds; ASTM D2240-91
Tensile Strength, Yield 14.5 MPa
2100 psi
ASTM D412-92
Elongation at Break 450 %
450 %
ASTM D412-92
200% Modulus 0.0121 GPa
1.76 ksi
ASTM D412-92
Tear Strength 31.6 kN/m
180 pli
Initial Tear Strength; ASTM D1004-93
Compression Set 64 %

@Temperature 70.0 °C
64 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746-79
Electrical Properties Metric English Comments
Dielectric Strength 20.4 kV/mm
518 kV/in
ASTM D149-93
Descriptive Properties Value Comments
Color Clear