Material Notes:
Texaco Cyngus Greases are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in two grades, Texaco Cyngnus Greases were developed for the food processing and canning industries.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 222662; MSDS Number: 8645
Physical Properties Metric English Comments
Viscosity Measurement 109
109
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1060 SUS
1060 SUS
See Note 3.
Saybolt Viscosity at 210°F 98 SUS
98 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 202 cSt
202 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 19.4 cSt
19.4 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Wear 0.440 mm
0.0173 in
Scar Diameter
Penetration P(60), 1/10 mm 280
280
Unknown Amount of Work, 25°C (77°F)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
See Note 2.
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
See Note 1.
Pour Point -13.0 °C
8.60 °F
See Note 3.
Flash Point 200 °C
392 °F
See Note 3.
Dropping Point 287 °C
549 °F
Descriptive Properties Value Comments
Color White
Texture Smooth, Buttery
Thickener, % 20.8
Polyurea Complex