Material Notes:
Description: OPTICOOL 570 is a high performance blend of synthetic and emulsion technology, OPTICOOL 570 formulation offer superior lubrication/cooling, corrosion inhibition, extreme pressure resistance, rancidity control and hard water stability. 570 is ideal for multi-task machining centers. The flexible technology and additive package arsenal allows for plant standardization of multi-machining fluidsProperties:Excellent Lubrication/Cooling PropertiesExcellent Foam ControlClean, Safe Work EnvironmentSuperior Heat DissipationExtreme Pressure CapabilityExcellent Hard Water StabilityReduces Mist and Inhalation HazardsResists Microbial AttackExcellent Corrosion ProtectionMild to the SkinSuggested uses:MillingTurningGrindingStampingDrawingBroachingDrillingReamingSawingTappingThreadingInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
pH 9.0
9.0
5% Concentrate
9.0 - 9.4
9.0 - 9.4
Concentrate
Viscosity Measure 22 cSt

@Temperature 40.0 °C
22 cSt

@Temperature 104 °F
Descriptive Properties Value Comments
Appearance Clear, amber
5% water
Composition 0.1
EP Non-Chlorinated
0.1
EP Chlorinated
Form Liquid Concentrate
Copyright © lookpolymers.com All Rights Reserved