Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® AC125G Acetal Copolymer, 25% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chase Plastics CP Pryme® AC125G Acetal Copolymer, 25% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Water Absorption 0.18 %
0.18 %
24 hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 128 MPa
18500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 164 °C

@Thickness 3.17 mm
327 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 163 °C

@Thickness 3.17 mm
325 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Users viewing this material also viewed the following: