3M 6035PC 12030 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series)

Category Polymer , Adhesive
Manufacturer 3M
Trade Name 6035PC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 6035PC 12030 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and sealing applications. Has excellent resistance to compression set and die cuts cleanly. 3M™ acrylic adhesive provides an excellent bond to various surfaces and has good shear strength at elevated temperatures. Available in 15 lb/ft3 and 20 lb/ft3 densities.Information provided by 3M
Physical Properties Metric English Comments
Water Absorption 4.0 %
4.0 %
ASTMD570
Mechanical Properties Metric English Comments
Elongation at Break 90 %
90 %
ASTMD3574-E Die E
Compressive Strength 2.10 MPa
305 psi
Force Deflection; ASTMD3574-D
Tear Strength 0.700 kN/m
4.00 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 107 °C
225 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month