Material Notes:
Micro-Melt® M-3 Class 2 alloy is a powder metal tungsten-molybdenum high-speed steel possessing the superior wear resistance characteristics required for difficult cutting operations. The advantages of Micro-Melt premium powder high speed steels include ease of grinding, response to heat treatment, more uniform structure, greater wear resistance and improved toughness. In addition, Carpenter's unique hot rolling and rotary forging capabilities impart minimal distortion characteristics to these alloys.Applications: Broaches, Form tools, Drills, Counterbores, Milling cutters, End mills, Chasers, Taps, Lathe tools, Planer tools, ReamersInformation provided by Carpenter Technology Corporation.Micro-Melt® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Specific Gravity 8.16 g/cc
8.16 g/cc
Mechanical Properties Metric English Comments
Hardness, Rockwell C 57 - 59
57 - 59
Tempered at 1150°F
65 - 66
65 - 66
As quenched
Modulus of Elasticity 207 GPa
30000 ksi
Izod Impact Unnotched 32.5 - 42.0 J
24.0 - 31.0 ft-lb
Component Elements Properties Metric English Comments
Carbon, C 1.25 %
1.25 %
Chromium, Cr 4.0 %
4.0 %
Iron, Fe 79.43 %
79.43 %
As Balance
Molybdenum, Mo 6.0 %
6.0 %
Sulfur, S 0.070 %
0.070 %
Tungsten, W 6.25 %
6.25 %
Vanadium, V 3.0 %
3.0 %