Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins IPETHENE® 600 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Carmel Olefins
Trade Name IPETHENE®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Carmel Olefins IPETHENE® 600 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
IPETHENE® 600 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits good stiffness and moderate melt flow rate. APPLICATIONS IPETHENE® 600 is used to produce lids, containers, toys, compounds, and masterbatches.
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ISO 1183-A
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.5 MPa
1520 psi
ISO 527-2
Tensile Strength, Yield 9.00 MPa
1310 psi
ISO 527-2
Elongation at Break 500 %
500 %
ISO 527-2
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C

@Load 1.02 kg
189 °F

@Load 2.25 lb
ISO 306
Users viewing this material also viewed the following: