Carlson 70 30 Cu Ni Copper-Nickel Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Nickel Alloy
Manufacturer Carlson
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Carlson 70 30 Cu Ni Copper-Nickel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionCarlson alloy 70 30 Cu Ni is a copper nickel alloy with excellent resistance to corrosion and erosion. It is strong and ductile. 70 30 Cu Ni is utilized in areas where high temperatures and pressures, combined with high velocities and turbulence are serious problems. It can be utilized up to 700°F for ASME code heat exchangers and unfired pressure vessels.70 30 Cu Ni exhibits outstanding resistance to general and impingent attack by clean sea water. It is, however, subject to bio-fouling at low velocities. 70 30 Cu Ni also has excellent resistance to attack by fresh water, boiler feedwater, and steam. It withstands the attack of phosphoric, sulfuric, and mild organic acids. It is attacked by chromic, hydrobromic, hydrochloric, and nitric acids. 70 30 Cu Ni is resistant to alkaline chlorides, chromates, nitrates and sulfates. It is, however, attacked by the cyanides and acid dichromates. 70 30 Cu Ni resists wet and dry chlorine, bromine, and carbon dioxide at ambient temperatures.Applications70 30 Cu Ni is widely used in marine service, tidewater power plants, desalinization plants, oil refineries, and in the chemical process industry. It is utilized extensively as a condenser and salt water tube and piping material for the U.S. Navy.Product applications include condenser, heat exchanger and distiller tubes, tube sheets and baffles, sale water piping, water boxes, tanks, vats, pressure vessels, process equipment, pumps and valves.Information provided by Carlson
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 310 MPa
<br>@Thickness >=63.5 mm
45000 psi
<br>@Thickness >=2.50 in
>= 345 MPa
<br>@Thickness <=63.5 mm
>= 50000 psi
<br>@Thickness <=2.50 in
Tensile Strength, Yield 124 MPa
<br>@Strain 0.200 %,<br> Thickness >=63.5 mm
18000 psi
<br>@Strain 0.200 %,<br> Thickness >=2.50 in
>= 138 MPa
<br>@Strain 0.200 %,<br> Thickness <=63.5 mm
>= 20000 psi
<br>@Strain 0.200 %,<br> Thickness <=2.50 in
Elongation at Break >= 35 %
>= 35 %
Modulus of Elasticity 152 GPa
22000 ksi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C
<br>@Temperature 20.0 - 300 °C
9.00 µin/in-°F
<br>@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C
0.0900 BTU/lb-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
Copper, Cu 64.39 - 70.6 %
64.39 - 70.6 %
Iron, Fe 0.40 - 1.0 %
0.40 - 1.0 %
Lead, Pb <= 0.020 %
<= 0.020 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 29 - 33 %
29 - 33 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Sulfur, S <= 0.020 %
<= 0.020 %
Zinc, Zn <= 0.50 %
<= 0.50 %