California Fine Wire Stablohm 650 Nickel Chromium Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer California Fine Wire
Trade Name Stablohm
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Stablohm 650 Nickel Chromium Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.41 g/cc
0.304 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 689 MPa
100000 psi
Annealed
1210 MPa
175000 psi
Stress relieved
1380 MPa
200000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 14.5 µm/m-°C

@Temperature 20.0 °C
8.06 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 11.3 W/m-K
78.4 BTU-in/hr-ft²-°F
Melting Point 1395 °C
2543 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Operating Temperature
Component Elements Properties Metric English Comments
Chromium, Cr 20 %
20 %
Nickel, Ni 80 %
80 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000108 ohm-cm
0.000108 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance 0.000085 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper +0.006