Cadi 10WA Tungsten Copper Alloy

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Cadi Company
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Cadi 10WA Tungsten Copper Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company.
Physical Properties Metric English Comments
Density 14.8 g/cc
0.535 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 104 - 110
104 - 110
Component Elements Properties Metric English Comments
Copper, Cu 25 %
25 %
Tungsten, W 75 %
75 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000573 - 0.00000688 ohm-cm
0.00000573 - 0.00000688 ohm-cm
Calculated from 25-30 %IACS