Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Nylon
Manufacturer CRP Technology
Trade Name Windform®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF CRP Technology Windform® LX 2.0 Polyamide Composite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability point of view. Windform® LX 2.0 is a new polyamide based material reinforced with new generation glass fiber system. The properties of Windform® LX 2.0 make it particularly suited for functional applications and finished complex parts. Windform® LX 2.0 is a naturally black material and is characterized by improved Ultimate Tensile Strength, increased stiffness as well as a high level of resistance to temperature, while providing an attractive surface finish. Windform® LX 2.0 also underlines its advantage towards Windform® GF, PRO and PRO B, with an excellent rate between quality and price. Windform® LX 2.0 is perfect to create functional prototypes or finished parts that require reliability, good temperature resistance and a captivating matte black color.Sample applications: There are several fields of application: covers, latching systems, air intake systems, connectors, applications for drivers cockpit (e.i. steering wheel-mounted paddle shifters), but also cooling/ducted fans, UAV structural components, sport functional prototypes, performing design parts and stiff pieces for packaging, and other applications in the naval and aerospace industries.Information provided by CRP Technology.
Physical Properties Metric English Comments
Density 1.311 g/cc
0.04736 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.9 MPa
8690 psi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 2.3 %
2.3 %
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 6.248 GPa
906.2 ksi
UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 92.2 MPa
13400 psi
UNI EN ISO 14125: 2000
Flexural Modulus 4.86 GPa
705 ksi
UNI EN ISO 14125: 2000
Charpy Impact Unnotched 1.814 J/cm²
8.633 ft-lb/in²
ISO 179-1:2007
Charpy Impact, Notched 0.437 J/cm²
2.08 ft-lb/in²
ISO 179-1:2007
Thermal Properties Metric English Comments
CTE, linear 36.3 µm/m-°C

@Temperature 60.0 - 110 °C
20.2 µin/in-°F

@Temperature 140 - 230 °F
X direction
118.4 µm/m-°C

@Temperature 60.0 - 110 °C
65.78 µin/in-°F

@Temperature 140 - 230 °F
Y direction
194.2 µm/m-°C

@Temperature 60.0 - 110 °C
107.9 µin/in-°F

@Temperature 140 - 230 °F
Z direction
Melting Point 180.0 °C
356.0 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 175.7 °C
348.3 °F
ASTM D648
Vicat Softening Point 177.8 °C
352.0 °F
10 N; ASTM D1525
Descriptive Properties Value Comments
Color Black
Surface Finish 1.5 Ra µm
After Finishing
7.5 Ra µm
After SLS Process