| Category | Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy |
| Manufacturer | CMW Inc. |
| Trade Name | THERMKON® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | CMW® THERMKON® 68 Tungsten Copper parts.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 16.31 g/cc | 0.5892 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell C | 25 | 25 | |
| Tensile Strength, Ultimate | 827 MPa | 120000 psi | |
| Tensile Strength, Yield | 724 MPa | 105000 psi | |
| Modulus of Elasticity | 248 GPa | 36000 ksi | |
| Flexural Modulus | 1.206 GPa | 174.9 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.50 µm/m-°C @Temperature 20.0 °C |
3.61 µin/in-°F @Temperature 68.0 °F |
|
| Specific Heat Capacity | 0.163 J/g-°C | 0.0390 BTU/lb-°F | |
| Thermal Conductivity | 167 W/m-K | 1160 BTU-in/hr-ft²-°F | |
| Melting Point | 1080 - 2610 °C | 1980 - 4730 °F | |
| Solidus | 1080 °C | 1980 °F | |
| Liquidus | 2610 °C | 4730 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 15 % | 15 % | |
| Tungsten, W | 85 % | 85 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00000493 ohm-cm | 0.00000493 ohm-cm | (35% IACS) |