Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONITE® 3W3 Tungsten Copper material ASTM B702

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name ELKONITE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONITE® 3W3 Tungsten Copper material ASTM B702.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
For arcing and current carrying electrical contacts, power transformer contacts, resistance welding electrodes.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 13.83 g/cc
0.4996 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Flexural Modulus 0.896 GPa
130 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 160 W/m-K
1110 BTU-in/hr-ft²-°F
Melting Point 1080 - 3410 °C
1980 - 6170 °F
Solidus 1080 °C
1980 °F
Liquidus 3410 °C
6170 °F
Component Elements Properties Metric English Comments
Copper, Cu 32 %
32 %
Tungsten, W 68 %
68 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000345 ohm-cm
0.00000345 ohm-cm
(50% IACS)