Buckeye Polymers BP PP 0015 R Blk Reprocessed Polypropylene, Unfilled

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Buckeye Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP PP 0015 R Blk Reprocessed Polypropylene, Unfilled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PP Homo BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds are utilized in this mineral reinforced polypropylene product to help meet the wide recycling requirements.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.1 MPa
3210 psi
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648