Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem TI4003F Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem TI4003F Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Extra High Izod Impact, Very High Flexural Modulus, Good Low Temperature Drop ImpactApplications: Suggested Uses Include Blow Molding, Extrusion, Profiles, PipeThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ASTM D785
Tensile Strength 29.0 MPa
4200 psi
2 in/min; ASTM D638
Elongation at Yield 10.5 %
10.5 %
2 in/min; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched NB
NB
ASTM D256A
Impact Test 48.8 J

@Temperature -29.0 °C
36.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Users viewing this material also viewed the following: