Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Bhansali
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D-955
Melt Flow 26 g/10 min

@Load 10.0 kg,
Temperature 220 °C
26 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D-785
Tensile Strength, Yield 37.3 MPa

@Thickness 3.20 mm
5400 psi

@Thickness 0.126 in
Type 1; 5mm/min; ASTM D638
Flexural Yield Strength 57.9 MPa

@Thickness 6.40 mm
8390 psi

@Thickness 0.252 in
ASTM D790
Flexural Modulus 2.16 GPa

@Thickness 6.40 mm
313 ksi

@Thickness 0.252 in
ASTM D790
Izod Impact, Notched 1.96 J/cm

@Thickness 6.40 mm
3.67 ft-lb/in

@Thickness 0.252 in
ASTM D256
2.25 J/cm

@Thickness 3.20 mm
4.22 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
Method A - Annealed; ASTM D-648
Vicat Softening Point 95.0 °C
203 °F
Method B; ASTM D-1525
Flammability, UL94 V-0
V-0
3.2 mm; Certified at 1.6 mm; UL-94
Users viewing this material also viewed the following: