Beijing Evergrow Resources PB-30 Glass Fiber Tissue

Category Ceramic , Glass , Glass Fiber
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources PB-30 Glass Fiber Tissue.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:Lightness, heat resisting, low thermal capacity and low thermal conductivity, soft and excellent fire-isolation. Anti-heat energy and heat stability.Anti-mildew, anti-insect, un-scattered and good stretching resistance.Excellent anti-ageing.Excellent sound absorbability, adsorption and filtering.It can be cut, sewn according to requirements and it's also easy to construct.Application:These products are widely used for wrapping material of all kinds of heat source (coal, electricity, oil, and gas) and heat-presentation of central air-conditioning pipelines.It can be used as the materials for heat-isolation and fire-resistance.It can be used as the materials for seal, sound absorption filtering and insulation.Excellent material for heat-conducting, heat-presentation.It can be used as materials for sound isolation, heat insulation and heat-resistance.It can also be used for touching fire and all kinds of flue in which the temperature is less than 600ºCInformation provided by Beijing Evergrow Resources.
Descriptive Properties Value Comments
Efficiency (%) 85
filter
Initial Resistance (Pa) 55
Precision (micron) 60
Tensile Strength at Yield (N/m) 60000
radial
60000
latitudinal
Width (mm) 600, 1000