| Category | Polymer , Thermoplastic , Nylon |
| Manufacturer | Beijing Evergrow Resources |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Beijing Evergrow Resources Glass Filled Nylon.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | GB1033 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 - 90 | 85 - 90 | GB3398 |
| Ball Indentation Hardness | 175 MPa | 25400 psi | GB3398 |
| Tensile Strength at Break | 130 - 150 MPa | 18900 - 21800 psi | GB/T 1040 |
| Elongation at Yield | <= 20 % | <= 20 % | GB/T 1040 |
| Modulus of Elasticity | 6.90 GPa | 1000 ksi | GB/T 1040 |
| Flexural Strength | 150 MPa | 21800 psi | GB9341 |
| Compressive Strength | 110 - 130 MPa | 16000 - 18900 psi | GB/T 1040 |
| Izod Impact, Notched (ISO) | 5.50 kJ/m² | 2.62 ft-lb/in² | GBT1043 |
| Coefficient of Friction | 0.45 | 0.45 | GB3360 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 25.0 µm/m-°C | 13.9 µin/in-°F | GB1036 |
| Melting Point | 260 °C | 500 °F | HG/T2235 |
| Heat Distortion Temperature | 150 °C | 302 °F | GB1634 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | Volume; GB1410 |
| Arc Resistance | 475 sec | 475 sec | ASTM D112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 1.65 - 1.83 % | 1.65 - 1.83 % | in air |
| 3.5 - 4.1 % | 3.5 - 4.1 % | in water |