BASF Ultramid® B40 01 PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B40 01 PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultramid B40 01 is a high viscosity, PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 9.5 %
9.5 %
ISO 62
Moisture Absorption at Equilibrium 2.6 %
2.6 %
23°C/50% R.H.; ISO 62
Relative Viscosity 4.0 cP
4.0 cP
ISO Test; 96 % SAV
Viscosity Test 250 cm³/g
250 cm³/g
Viscosity number
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min
Descriptive Properties Value Comments
Color Natural
Commercial Status North America and Europe
FDA 21 CFR 177.1500
Impact Modified No
Primary Processing Technique Film Extrusion