BASF Ultramid® A3WG7 HP BK 20560 35% Glass Filled PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3WG7 HP BK 20560 35% Glass Filled PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade for technical articles such as gearwheels, solenoid valve housings, cable contacts and components for automotive gear shifting systems.Information provided by BASF