Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SYL-OFF® PMCPSL 9156 Release Modifier

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® PMCPSL 9156 Release Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Syl-Off® SL 9156 Release Modifier is one component of a multi-component silicone release system designing for coating on polyester substrates.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Users viewing this material also viewed the following: