BASF Ultradur B 4300 G6 BK5110 30% Glass Filled PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultradur B
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur B 4300 G6 BK5110 30% Glass Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultradur B 4300 G6 BK5110 is an easy flowing, pigmented black, injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
Water Absorption 0.20 %
0.20 %
24 hour; ISO Test
0.40 %
0.40 %
ISO 62
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C/50% R.H.; ISO 62
Viscosity Test 102 cm³/g
102 cm³/g
Viscosity number
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM Data; MD
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 135 MPa
19600 psi
5mm/min; ISO 527
Elongation at Break 2.9 %
2.9 %
5mm/min; ISO 527
Tensile Modulus 10.4 GPa
1510 ksi
1mm/min; ISO 527
Flexural Modulus 8.82 GPa
1280 ksi
ISO Data
Izod Impact, Notched (ISO) 8.30 kJ/m²
3.95 ft-lb/in²
ISO Test
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min
223 °C
433 °F
ASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 197 °C
387 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Descriptive Properties Value Comments
Color BK5110
Commercial Status North America and Europe
Form Pellets
Impact Modified No
Primary Processing Technique Injection Molding
Special characteristic Heat stabilized or stable to heat
Light stabilized or stable to light
Lubricant
U.V. stabilized or stable to weather