Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ecoflex® 1200 F Blend Biodegradable Polyester

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP
Manufacturer BASF
Trade Name Ecoflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ecoflex® 1200 F Blend Biodegradable Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film extrusion is a particular area where Ecoflex® F shows well-balanced processing properties, and the resin can also be used in extrusion coating applications. Ecoflex® F requires no predrying prior to extrusion. Antiblock and Slip additives are recommended and are available from BASF.Applications: Ecoflex® F Blend 1200 can be used for applications such as compost bags, trash bags, carrier bags, bags for fruits and vegetables, general packaging films, agricultural films, and laminating films for trays made from natural materials.Information provided by BASF
Physical Properties Metric English Comments
Density 1.25 - 1.27 g/cc
0.0452 - 0.0459 lb/in³
ISO 1183
Melt Flow 2.7 - 4.9 g/10 min
2.7 - 4.9 g/10 min
ISO 1133
Surface Tension 34 dynes/cm
34 dynes/cm
Mechanical Properties Metric English Comments
Hardness, Shore D 32
32
ISO 868
Tensile Strength 34.0 MPa
4930 psi
ISO 527
Film Elongation at Break, MD 560 %
560 %
ISO 527
Film Elongation at Break, TD 700 %
700 %
ISO 527
Dart Drop Total Energy 2.40 J/cm
0.00450 ft-lb/mil
DIN 53373
Thermal Properties Metric English Comments
Melting Point 110 - 120 °C
230 - 248 °F
DSC
Vicat Softening Point 80.0 °C
176 °F
A/50; ISO 306
Optical Properties Metric English Comments
Transmission, Visible 82 %
82 %
ASTM D1003
Descriptive Properties Value Comments
Commercial Status Europe