| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Capron® B73QP Nylon 6 (DAM)
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Volatiles | 0.80 % | 0.80 % | Extractable |
| Water Absorption | 1.6 % | 1.6 % | 24 hr.; ISO 62 |
| 9.5 % | 9.5 % | ISO 62 | |
| Moisture Absorption at Equilibrium | 0.080 % | 0.080 % | ASTM D570 |
| 2.7 % | 2.7 % | 23°C/50% R.H.; ISO 62 | |
| Oxygen Transmission Rate | 40.3 cc/m²/day | 2.60 cc/100 in²/day | |
| Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
| Carbon Dioxide Transmission | 72.8 cc-mm/m²-24hr-atm | 185 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
| Viscosity Measurement | 3.0 | 3.0 | Relative Viscosity (96% SAV) |
| 3.1 | 3.1 | Relative Viscosity (95% SAV) | |
| 3.2 | 3.2 | Relative Viscosity (98% SAV) | |
| 73 | 73 | Formic Acid; ASTM D789 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 80.0 MPa | 11600 psi | 2 in/min; ASTM D638 |
| Flexural Strength | 100 MPa | 14500 psi | ASTM D790 |
| Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
| Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | 10 K/min |
| 220 °C | 428 °F | ASTM D3418 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Unfilled | |
| Color | Natural | |
| Commercial Status (March 2007) | Active America | |
| FDA | 21 CFR 177.1500 | |
| Impact Modified | No | |
| Primary Processing Technique | Film Extrusion |