Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 18860 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 18860 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame retardant jacketing compound recommended for a maximum service temperature rating of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.40 - 1.44 g/cc
1.40 - 1.44 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 83 - 89
83 - 89
delayed; ASTM D-2240
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D-638
Elongation at Yield 265.7 %
265.7 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
310 %
310 %
ASTM D-638
100% Modulus 0.0110 GPa
1.60 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 28.5 %
28.5 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F
Users viewing this material also viewed the following: