Assab Steels EM33 Steel for Plastic Molds

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer Assab Steels
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Assab Steels EM33 Steel for Plastic Molds.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Prehardened plastic mould and holder steel with excellent toughness and machinability.Applications: Plastic and rubber moulds, support plates and constructional parts. Stripper plates in blanking application. Holders/bolsters for plastic moulds and die casting dies.
Mechanical Properties Metric English Comments
Hardness, Brinell 280 - 340
280 - 340
hardness supplied.