Ashley Polymers Ashlene® 528L-25G Nylon 66, 25% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528L-25G Nylon 66, 25% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose glass reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 166 MPa
24100 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 251 °C
484 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 246 °C
475 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
ASTM D648