| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant | 
| Manufacturer | Ashley Polymers | 
| Trade Name | Ashlene® | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Ashley Polymers Ashlene® 528BR-WO Nylon 66.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 | 
| Water Absorption | 1.1 % | 1.1 % | ASTM D570 | 
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 119 | 119 | ASTM D785 | 
| Tensile Strength, Ultimate | 68.0 MPa | 9860 psi | ATSM D638 | 
| Elongation at Break | 20 % | 20 % | ASTM D638 | 
| Flexural Strength | 101 MPa | 14600 psi | ASTM D790 | 
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 | 
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 254 °C | 489 °F | ASTM D3418 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 207 °C | 405 °F | ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 | 
| Flammability, UL94 |           V-0                     @Thickness 1.80 mm  | 
                  V-0                     @Thickness 0.0709 in  |