Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Norton® V760 High Density Vibration

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® V760 High Density Vibration.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Seals and Dampens Vibration: Norseal® V760 is a closed-cell PVC foam sealant with a pressure-sensitive adhesive on one side. Its high-density structure and multitude of tiny cells act like shock absorbers to seal and dampen vibration. Firm, High Density Foam for Positive Seals: This shock-absorbing feature makes Norseal V760 ideal for die-cut applications and metal-to-metal sealing. Versatile and easy to use, Norseal V760 is designed to produce a positive seal in mechanically fastened assemblies with as little as 30 percent compression. Conformable and Dimensionally Stable: Norseal V760 provides excellent conformability to curved and irregular shapes. It is resistant to weather, fungi and oxidation, ensuring a long sealing life. In addition, Norseal V760 is dimensionally stable. It will not drip, ooze or run under compression, and remains flexible at low temperatures. Pressure Sensitive Adhesive: The aggressive pressure-sensitive adhesive on one side of Norseal V760 facilitates high-speed application. The easy-peel paper liner eliminates stretching during installation, and removes easily after application. Norseal V760 series is available in gray. For specific low energy plastics, a specially formulated adhesive, "LE" is available.FEATURES/BENEFITS:Dimensionally stable under compressionGood abrasion resistanceDesign facilitates high-speed applicationLiner removes easily after applicationResistant to wether, fungi and oxidationLow water absorption for long sealing lifeProvides insulating propertiesApplications: Truck trailer joint seals, door frame assemblies, concrete forms, export container seals, die-cut gaskets, roof sealing for parapets, duct seals, appliance seals, truck cab overlap seals. All data based on a 0.125 inch test sample.(Available in multiple thicknesses.) Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 0.238 g/cc
0.00860 lb/in³
ASTM D1667
Water Absorption 3.0 %
3.0 %
% by volume; NTP-35
Mechanical Properties Metric English Comments
Hardness, Shore OO 45
45
ASTM D2240
Tensile Strength, Yield 0.379 MPa
55.0 psi
ASTM D-412 (Die A)
Elongation at Break 140 %
140 %
ASTM D-412 (Die A)
Compressive Strength 0.0234 MPa
3.40 psi
Compression Deflection, Compressed to 30%.; ASTM D1667
Compressive Modulus 0.0000496 GPa
0.00720 ksi
Force to Compress, Value for 30% compression.; ASTM D1667
Compression Set 4.0 %
4.0 %
Constant Deflection, Compressed to 30%.; Norton Test Procedure 37
Thermal Properties Metric English Comments
Thermal Conductivity 0.0432 W/m-K
0.300 BTU-in/hr-ft²-°F
ASTM C-518
Maximum Service Temperature, Air 71.1 °C
160 °F
Minimum Service Temperature, Air -26.1 °C
-15.0 °F
Descriptive Properties Value Comments
Color Gray