Material Notes:
Polybutadiene Rubber (High cis BR)Characteristics: KBR 31 contains an aromatic oil additive. Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solution polymerization, and it is classified to High cis BR and Low cis BR according to the cis-1,4 content. High cis BR containing over 94% cis-1,4 is superior in abrasion resistance, elasticity, age resistance and water resistance. As the secondary transition temperature is about -100? low, it is most widely utilized together with SBR.Applications: Conveyor belting, tires (superior for snow tire tread).Additional Notes: Extender Oil: 37.5; AromaticStabilizer: Non-Pollutingcis-1,4 Contents: 95%Volatile Matter: 0.3%Ash Content: 0.1%This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Not Compounded
Mooney Viscosity 35

@Temperature 100 °C
35

@Temperature 212 °F
Raw; ML1+4
71

@Temperature 100 °C
71

@Temperature 212 °F
Compounded; ML1+4; KOSYN KBR31 137.5, ZnO 3, Stearic Acid 2, HAF Black (IRB#6) 82.5, Accelerator TBBS 1.24, Sulfur 1.5 Total: 227.7
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
Cured; JIS-A
Tensile Strength, Ultimate 18.8 MPa
2730 psi
Cured
Elongation at Break 640 %
640 %
Cured
300% Modulus 0.00804 GPa
1.17 ksi
Cured
Rebound 47 %
47 %
ASTM
Flex Crack Resistance 6000
6000
De Mettia Flexometer Cut Growth: 2mm --> 15mm, Flexes
Tear Strength 69.6 kN/m
398 pli
B-type
Abrasion 0.0040
0.0040
Akron type Tester (cc/1000rev)
Compression Set 4.0 %
4.0 %
Permanent Set
13 %

@Temperature 70.0 °C
13 %

@Temperature 158 °F
70°C / 22 hrs, 25%, def