Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.5 MPa | 1670 psi | |
Elongation at Break | 200 % | 200 % | IEC60811-1-1 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Index | 45 % | 45 % |