AlphaGary Megolon™ HF 8110 LD UV Low Smoke Halogen Free

Category Polymer , Thermoplastic
Manufacturer AlphaGary
Trade Name Megolon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Megolon™ HF 8110 LD UV Low Smoke Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose sheathing compound with good mechanical, processing properties and reduced die drool. UV resistant. Application examples include Data Cables, Optical Cables.
Mechanical Properties Metric English Comments
Tensile Strength 11.0 MPa
1600 psi
Elongation at Break 150 %
150 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 34 %