Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) |
Manufacturer | AlphaGary |
Trade Name | Garaflex™ O |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary Garaflex™ O 9940 DWN-R Olefinic Thermoplastic Elastomer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 44 - 53 | 44 - 53 | |
Tensile Strength | 15.2 MPa | 2200 psi | |
Elongation at Break | 550 % | 550 % | ASTM D412 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Oxygen Index | 35 % | 35 % |