Category | Polymer , Thermoplastic , Elastomer, TPE |
Manufacturer | AlphaGary |
Trade Name | Evoprene™ CE |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary Evoprene™ CE 6186 Thermoplastic Elastomer.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.10 g/cc | 1.10 g/cc | ISO 2781 |
Viscosity Measurement | 17 @Temperature 150 °C |
17 @Temperature 302 °F |
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 60 | 60 | ISO 868 |
Tensile Strength | 4.80 MPa | 696 psi | ISO 37 |
Elongation at Break | 550 % | 550 % | ISO 37 |
100% Modulus | 0.00220 GPa | 0.319 ksi | ISO 37 |
Tear Strength | 27.0 kN/m | 154 pli | ISO 34-B |
Compression Set | 28 % @Temperature 23.0 °C, Time 259000 sec |
28 % @Temperature 73.4 °F, Time 72.0 hour |
ISO 815 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Bonds with | Polypropylene | |
Transparency | Opaque |