Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer APA - Advanced Polymer Alloys
Trade Name DURACRYN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DURACRYN 8060 NC/BK Thermoplastic Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 51
51
Time of 15 seconds; ASTM D2240
59
59
Instantaneous; ASTM D2240
Tensile Strength, Ultimate 10.3 MPa
1500 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412
100% Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Graves Tear Strength 28.0 kN/m
160 pli
Die C; ASTM D624
Compression Set 64 %

@Temperature 70.0 °C
64 %

@Temperature 158 °F
Method B, 22 hours; ASTM D395
Tensile Set 9.0 %
9.0 %
ASTM D412