| Category | Polymer , Thermoplastic , Nylon |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adell ZS-30 Nylon/Olefin Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 51.0 MPa | 7400 psi | ASTM D638 |
| Elongation at Break | 50 % | 50 % | ASTM D638 |
| Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
| Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
| Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
| 0.587 J/cm <br>@Temperature -40.0 °C |
1.10 ft-lb/in <br>@Temperature -40.0 °F |
ASTM D256 | |
| Izod Impact, Unnotched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
| 8.01 J/cm <br>@Temperature -40.0 °C |
15.0 ft-lb/in <br>@Temperature -40.0 °F |
ASTM D256 | |
| Gardner Impact | 1.10 J | 0.811 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 48.9 °C | 120 °F |