Lubriplate H0-4 Petroleum-Based Heavy-Duty Hydraulic Oil

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate H0-4 Petroleum-Based Heavy-Duty Hydraulic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High aniline points ensure long seal life with fewer leaks. They can withstand elevated temperatures & high pressures over extended drain intervals. High natural V.I. provides stable viscosities over a wide temperature range. Excellent ISO cleanliness ratings. HO Series Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 101
101
Viscosity Index
150
150
ISO Grade
Saybolt Viscosity at 100°F 840 SUS
840 SUS
Saybolt Viscosity at 210°F 83 SUS
83 SUS
Kinematic Viscosity at 40°C (104°F) 162 cSt
162 cSt
Kinematic Viscosity at 100°C (212°F) 16 cSt
16 cSt
Thermal Properties Metric English Comments
Pour Point -17.8 °C
0.000 °F
Flammability Test 525
525
[°F] Fire Point
Flash Point 243 °C
470 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 90
SAE No. 40