| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid) Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | initial |
| Malvern Minerals Nylon with Novakup® L-337 Silane-Treated Quartz Filler Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in nylon. Th.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Kostat ICP-STAT ICS-1003 PS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Kostat ICP-STAT ICS-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| KYDEX® 2200LT Thermoplastic Sheet for Mass Transit Applications Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graf.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Kostat ICP-STAT ICD-1003 PS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Kostat ICP-STAT ICD-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Techmer ES Electrablend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9874105Information provided by TP Composites, Inc. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP (Asia Pacific) LNP* Thermocomp* MX92284 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP LNP* THERMOCOMP* MX92284 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Saint-Gobain Meldin® 7211 Isostatically Molded Graphite and PTFE Filled Polyimide Finished parts and basic shapes made from 10% by weight PTFE and 15% by weight graphite filled polyimide material for applications requiring a very low coefficient of friction and self-lubricating p.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Adell YS-10 PC Alloy |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D-790 |
| Axiall 3152 Rigid PVC, Extrusion Georgia Gulf 3152 is a twin screw powder blend NSF approved for the extrusion of potable water and drain waste and vent pipe application.Information provided by Georgia GulfGeorgia Gulf became Axial.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | |
| Abatron AboCast 8503-5/AboCure 8503-5 Colorless Epoxy AboCast 8503-5/AboCure 8503-5 is a faster hardening, colorless epoxy casting compound used for small castings and decoupage. It is a good choice for small castings, especially for analytical purpose.. |
|||
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D-790 |
| Axiall 7407 Rigid PVC, Extrusion Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||